The use of SSA fractionation to detect changes in the molecular structure of model ethylene–butene copolymers modified by peroxide crosslinking

Four model ethylene–butene copolymers of different molecular weights modified with various concentrations of peroxide were analyzed by a DSC based successive self annealing method. The original copolymers had the same intra and intermolecular homogeneous branching distribution along the linear chain...

Descripción completa

Detalles Bibliográficos
Autores: Pérez, Claudio Javier, Villarreal, Norky, Pastor, Jose Maria, Failla, Marcelo Daniel, Valles, Enrique Marcelo, Carella, Jose Maria
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2009
País:Argentina
Institución:Consejo Nacional de Investigaciones Científicas y Técnicas
Repositorio:CONICET Digital (CONICET)
Idioma:inglés
OAI Identifier:oai:ri.conicet.gov.ar:11336/35063
Acceso en línea:http://hdl.handle.net/11336/35063
Access Level:acceso abierto
Palabra clave:Ethylene–Butene Copolymers
Organic Peroxide
Crosslinking
Successive Self-Nucleation And Annealing
https://purl.org/becyt/ford/2.4
https://purl.org/becyt/ford/2
Descripción
Sumario:Four model ethylene–butene copolymers of different molecular weights modified with various concentrations of peroxide were analyzed by a DSC based successive self annealing method. The original copolymers had the same intra and intermolecular homogeneous branching distribution along the linear chains with approximately 2.4% mol of ethyl branches. The copolymers with average molecular weights of 29,000, 45,000, 81,000 and 125,000 g/mol were modified with different amounts of 2,5-dimethyl-2,5-di(tert-butyl peroxy)-hexane (DBPH) as a crosslinking initiator. The molecular changes induced by the reaction with the peroxide affect the semicrystalline structure of the material. Variations in the crystal thickness distributions of the material as a consequence of the modification are related to the peroxide induced free radical reactions.